Volume 4, Issue 5 1300815
Full Paper

Coated Lithium Powder (CLiP) Electrodes for Lithium-Metal Batteries

Jennifer Heine

Jennifer Heine

MEET Battery Research Center, Corrensstrasse 46, 48149 Münster, Germany

Search for more papers by this author
Steffen Krüger

Steffen Krüger

MEET Battery Research Center, Corrensstrasse 46, 48149 Münster, Germany

Search for more papers by this author
Christoph Hartnig

Christoph Hartnig

Rockwood Lithium GmbH, Trakehner Str. 3, 60487 Frankfurt am Main, Germany

Search for more papers by this author
Ulrich Wietelmann

Ulrich Wietelmann

Rockwood Lithium GmbH, Trakehner Str. 3, 60487 Frankfurt am Main, Germany

Search for more papers by this author
Martin Winter

Martin Winter

MEET Battery Research Center, Corrensstrasse 46, 48149 Münster, Germany

Search for more papers by this author
Peter Bieker

Corresponding Author

Peter Bieker

MEET Battery Research Center, Corrensstrasse 46, 48149 Münster, Germany

E-mail: [email protected]Search for more papers by this author
First published: 18 November 2013
Citations: 166

Abstract

Safety issues caused by the metallic lithium inside a battery represent one of the main reasons for the lack of commercial availability of rechargeable lithium-metal batteries. The advantage of anodes based on coated lithium powder (CLiP), compared to plain lithium foil, include the suppression of dendrite formation, as the local current density during stripping/plating is reduced due to the higher surface area. Another performance and safety advantage of lithium powder is the precisely controlled mass loading of the lithium anode during electrode preparation, giving the opportunity to avoid Li excess in the cell. As an additional benefit, the coating makes electrode manufacturing safer and eases handling. Here, electrodes based on coated lithium powder electrodes (CLiP) are introduced for application in lithium-metal batteries. These electrodes are compared to lithium foil electrodes with respect to cycling stability, coulombic efficiency of lithium stripping/plating, overpotential, and morphology changes during cycling.